Polymer Property : Izod Impact, Notched = 33.7 ft-lb/in
Polymer Property :
Izod Impact, Notched =
33.7 ft-lb/in
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Notched
18.0
J/cm
33.7
ft-lb/in
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass
Data provided by the manufacturer, Owens Corning.