Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.160 - 33.0 J/cm | 0.300 - 61.8 ft-lb/in | Average value: 3.38 J/cm Grade Count:677 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |