Mechanical Properties Metric English Comments
Izod Impact, Notched 1.99 J/cm
3.73 ft-lb/in
ASTM D256
Omni Plastics OmniTuff™ CPP GRC43 Copolymer Polypropylene Glass Reinforced
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..