Mechanical Properties Metric English Comments
Izod Impact, Notched 23.5 J/cm
44.0 ft-lb/in
ASTM D256
Quantum Composites LYTEX® 4084 63% Glass Fiber Reinforced Epoxy SMC
LYTEX 4084 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention ..
Izod Impact, Notched 23.5 J/cm
44.0 ft-lb/in
ASTM D256A
DSM Somos® 14120 Water-resistant resin for stereolithography, White
DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p..