Mechanical Properties Metric English Comments
Izod Impact, Notched 22.0 J/cm

@Temperature 23.0 °C
41.2 ft-lb/in

@Temperature 73.4 °F
ISO 180
LyondellBasell Astryn EPF30U Polypropylene Copolymer
Key Features: medium melt flow, medium modulus, UV-stabilized, polypropylene copolymer, high impact strength, excellent processabilityApplications: door and luggage compartment scruff plates, seat t..