Izod Impact, Notched 10.94 J/cm
20.50 ft-lb/in
ASTM D256
Cresset Powers Cress-Alon™ NE6040-ST 4% Nano Clay Loaded, 6.0 r.v. Super Tough Grade Nylon 6, 50% RH
Surpasses super tough neat resins in strength, heat resistance, and hardness.Information provided by Cresset Powers Ltd.