Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.82 J/cm | 5.28 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Izod Impact, Notched | 2.82 J/cm | 5.28 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |