Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.59 J/cm | 4.85 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Izod Impact, Notched | 2.59 J/cm | 4.85 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer DescriptionPolyfort® FPP 3459 is a 30% glass filled copolymerInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 2.59 J/cm | 4.85 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer DescriptionPolyfort® FPP 3459 is a 30% glass filled copolymerInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 2.59 J/cm | 4.85 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer DescriptionPolyfort® FPP 3459 is a 30% glass filled copolymerInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 2.59 J/cm | 4.85 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer DescriptionPolyfort® FPP 3459 is a 30% glass filled copolymerInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 2.59 J/cm | 4.85 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer DescriptionPolyfort® FPP 3459 is a 30% glass filled copolymerInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 2.59 J/cm | 4.85 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer DescriptionPolyfort® FPP 3459 is a 30% glass filled copolymerInformation provided by A. Schulman. |