Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.40051 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.74746 - 1.28136 J/cm

@Temperature -40.0 - -40.0 °C
1.4003 - 2.40051 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.85 J/cm Grade Count:3
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Notched 0.74746 - 1.28136 J/cm

@Thickness 3.17 - 3.17 mm
1.4003 - 2.40051 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.85 J/cm Grade Count:3
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..