Mechanical Properties Metric English Comments
Izod Impact, Notched 1.228 J/cm

@Temperature 23.0 °C
2.301 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Ovation Polymers Opnyl OP66GF50 Nylon 66
Nylon 66-Glass reinforced(50%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
Izod Impact, Notched 1.228 J/cm
2.301 ft-lb/in
ASTM D256
Petromont 1100 High Density Polyethylene Resin
Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b..