Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched | 2.20 J/cm @Thickness 3.17 mm |
4.12 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® 228 Specialty, High Productivity
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
IDI Composites 44-1 Thermoset Polyester, Molding Multi-purpose medium strength material with excellent moldability and low cost.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature -30.0 °C |
4.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature 23.0 °C |
4.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB840 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature 23.0 °C |
4.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A30N02 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ISO 180 |
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature 23.0 °C |
4.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PAS701 ASA, UV Stabilized UV stabilized general purpose injection molding ASAInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM-D256 |
Braskem GM5010T2 HDPE High Density Extrusion Polyethylene GM5010T2 is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes. It is produced with bimodal technology and has high molar mass. It shows high mechanical.. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
ALM PA 650 Nylon 12 SLS Prototyping Polymer Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines.. |
|||
Izod Impact, Notched | 2.20 J/cm @Temperature 23.0 °C |
4.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A40B01 Nylon 66, 40% Long Fiber A 40% long fiber glass reinforced black nylon 6.6 heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |