Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.910 - 1.17 J/cm @Thickness 6.35 mm |
1.70 - 2.19 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ MP-20GF/15T Modified PPO - 20% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |