Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.103 J/cm | 2.066 ft-lb/in | ASTM D256A |
Resinoid 2002-4 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Izod Impact, Notched | 1.103 J/cm | 2.066 ft-lb/in | ASTM D256A |
Resinoid 2020 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |