Izod Impact, Notched 1.55 - 96.0 J/cm
2.90 - 180 ft-lb/in
Average value: 26.0 J/cm Grade Count:4
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..