Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.1356 - 9.12969 J/cm @Temperature 0.000 - 0.000 °C |
4.0009 - 17.1037 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 5.63 J/cm Grade Count:2 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 2.1356 - 9.12969 J/cm @Diameter 6.35 - 6.35 mm |
4.0009 - 17.1037 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 5.63 J/cm Grade Count:2 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |