Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |