Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.240 - 7.74 J/cm | 0.450 - 14.5 ft-lb/in | Average value: 0.842 J/cm Grade Count:66 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |