Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.10 - 7.36782 J/cm @Temperature -40.0 - 149 °C |
2.06 - 13.8029 ft-lb/in @Temperature -40.0 - 300 °F |
Average value: 3.97 J/cm Grade Count:2 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |