Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Asia Pacific) 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East) 19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |