Mechanical Properties Metric English Comments
Izod Impact, Notched 12.3 J/cm
23.0 ft-lb/in
ASTM D256
Sumitomo Bakelite North America EM 7302LD-2 Long Glass Fiber Reinforced Epoxy
EM 7302LD-2 is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirabl..
Izod Impact, Notched 12.3 J/cm
23.0 ft-lb/in
ASTM D256
Cheng Yu Plastic ML1230 PC/PTFE, 30% Glass
Copyright © lookpolymers.com All Rights Reserved