Polymer Property : Izod Impact, Notched = 11.5 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.14 J/cm

@Temperature -30.0 °C
11.5 ft-lb/in

@Temperature -22.0 °F
0.125 in; ASTM D256
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Izod Impact, Notched 6.14 J/cm

@Temperature -30.0 °C
11.5 ft-lb/in

@Temperature -22.0 °F
0.125 in; ASTM D256
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Izod Impact, Notched 6.14 J/cm
11.5 ft-lb/in
73°F, 0.125 in.; ASTM D256
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
Izod Impact, Notched 6.15 J/cm
11.5 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE
LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass.
Izod Impact, Notched 6.15 J/cm

@Temperature 23.0 °C
11.5 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE)
LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 6.14 J/cm

@Temperature 22.8 °C
11.5 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced
Data provided by Clariant Masterbatches