Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.62 J/cm @Temperature 23.0 °C |
19.90 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66
(Unverified Data**) Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers |