Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.13 J/cm | 18.98 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527LD Nylon 66 A very high impact, slightly lubricated nylon resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 10.13 J/cm | 18.98 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527LDS Nylon 66 A very high impact, slightly lubricated and heat stabilized nylon resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 10.13 J/cm | 18.98 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527LDW Nylon 66 A specialized nylon with very high impact resistance.Data provided by the manufacturer |