Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.83 J/cm @Temperature 23.0 °C |
3.43 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Lene™ H5211PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |