Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.816 J/cm @Thickness 3.17 mm |
3.402 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-0120B GF15 Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |