Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.30 - 1.57 J/cm | 2.44 - 2.94 ft-lb/in | Average value: 1.42 J/cm Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |