Izod Impact, Notched 0.80085 - 2.6695 J/cm

@Temperature -29.0 - -28.9 °C
1.5003 - 5.0011 ft-lb/in

@Temperature -20.2 - -20.0 °F
Average value: 1.43 J/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..