Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.774 J/cm | 1.45 ft-lb/in | ASTM D256 |
Ovation Polymers RIGITRON 20443 GF PBT, 43% Glass Reinforced PBT - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco.. |
|||
Izod Impact, Notched | 0.774 J/cm | 1.45 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® RMC-30 30% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Izod Impact, Notched | 0.775 J/cm | 1.45 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FR200GV20 Flame Retardant Nylon 66, 20% Glass Fiber |