Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.29 J/cm | 2.41 ft-lb/in | ASTM D256 |
Omni Plastics OmniTuff™ HPP GRC40 Homopolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Izod Impact, Notched | 1.29 J/cm | 2.42 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12 LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Notched | 1.29 J/cm | 2.41 ft-lb/in | |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |
|||
Izod Impact, Notched | 1.29 J/cm | 2.42 ft-lb/in | ASTM D256 |
Cheng Yu Plastic A703G2 ABS 20% Glass Fiber Reinforced |