Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.282 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.402 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS 3500 EF-Low Gel Extrusion Grade, Low Gel Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |