Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.210 - 0.64068 J/cm @Diameter 6.35 - 6.35 mm |
0.393 - 1.2003 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.330 J/cm Grade Count:10 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.210 - 0.64068 J/cm @Temperature 0.000 - 0.000 °C |
0.393 - 1.2003 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.330 J/cm Grade Count:10 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |