Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 0.6401 J/cm | >= 1.199 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |