Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.475 J/cm @Temperature -40.0 °C |
0.890 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Izod Impact, Notched | 0.475 J/cm @Temperature -40.0 °C |
0.890 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |