Polymer Property : Izod Impact, Notched = 0.730 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.390 J/cm
0.730 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp SRF 9702/C Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Medium Impact Resistance Uses: Electrical/Electronic Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Izod Impact, Notched 0.390 J/cm
0.730 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp SRP 9613 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex
Izod Impact, Notched 0.390 J/cm
0.730 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp DBS 8615 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex