Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.726 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.36 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.726 J/cm | 1.36 ft-lb/in | ASTM D256 |
Cheng Yu Plastic PP238G3 Polypropylene, 30% Glass Fiber |
|||
Izod Impact, Notched | 0.726 J/cm | 1.36 ft-lb/in | |
BCC Products MB 8250 Aluminum Board MB 8250 is an aluminum filled product that is dimensionally stable and exhibits great machinable properties. Features: excellent machineability, low dust emission, no shrinkage, low moisture absorp.. |
|||
Izod Impact, Notched | 0.726 J/cm | 1.36 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® TFIPP 2010 High Impact Talc Filled Polypropylene AAROPRENE® TFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |