Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.382 J/cm | 0.716 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 0.382 J/cm | 0.716 ft-lb/in | ASTM D256 |
Asia Technology Pioneers CAP 102 PP Nanocomposite Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di.. |
|||
Izod Impact, Notched | 0.382 J/cm | 0.716 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® N6000FR Nanoclay 4% Flame Retardant Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |