Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 0.646 J/cm | >= 1.21 ft-lb/in | ASTM D256 |
Buckeye Polymers BP PPC 0218-22 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance. Meets or exceeds all properties associated with GMP.PP.086R.Product Featur.. |