Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.588399 - 0.686465 J/cm @Temperature -30.0 - -30.0 °C |
1.10231 - 1.28603 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.826 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.588399 - 0.686465 J/cm @Thickness 3.17 - 6.35 mm |
1.10231 - 1.28603 ft-lb/in @Thickness 0.125 - 0.250 in |
Average value: 0.826 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.588399 - 5338.47 J/cm @Temperature -40.0 - -20.0 °C |
1.10231 - 10001.1 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 1.52 J/cm Grade Count:22 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 0.588399 - 5338.47 J/cm @Thickness 3.17 - 6.40 mm |
1.10231 - 10001.1 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 1.52 J/cm Grade Count:22 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 0.588399 - 1.49492 J/cm @Temperature -30.0 - -20.0 °C |
1.10231 - 2.80060 ft-lb/in @Temperature -22.0 - -4.00 °F |
Average value: 0.752 J/cm Grade Count:5 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Izod Impact, Notched | 0.588399 - 1.49492 J/cm @Thickness 3.17 - 6.40 mm |
1.10231 - 2.80060 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 0.752 J/cm Grade Count:5 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |