Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.533 J/cm | 0.999 ft-lb/in | ASTM D412 |
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Izod Impact, Notched | 0.533 J/cm | 0.999 ft-lb/in | ASTM D412 |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |