Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.205 J/cm | 0.384 ft-lb/in | ASTM D256 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Izod Impact, Notched | 0.205 J/cm | 0.384 ft-lb/in | ASTM D256 |
Plenco 3356 Phenolic, Granular, Transfer Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |