Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.375 J/cm | 0.703 ft-lb/in | ASTM D256 |
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Izod Impact, Notched | 0.375 J/cm | 0.703 ft-lb/in | ASTM D256 |
RedEye On Demand VeroWhite PolyJet Resin White for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |