Izod Impact, Notched 0.373 J/cm
0.698 ft-lb/in
ASTM D256
E-Polymers SEPAZ® N2020F Nanoclay 2% Fast cycle time Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Izod Impact, Notched 0.373 J/cm
0.698 ft-lb/in
ASTM D256
Cheng Yu Plastic FV30G20 POM, 20% Glass Fiber
Izod Impact, Notched >= 0.373 J/cm

@Thickness 6.35 mm
>= 0.698 ft-lb/in

@Thickness 0.250 in
ASTM D256
Gromax CCP PBT 3010-104 10% Glass Fiber Filled
Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent..