Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 0.343233 J/cm @Temperature -30.0 - -10.0 °C |
>= 0.643016 ft-lb/in @Temperature -22.0 - 14.0 °F |
Average value: 0.537 J/cm Grade Count:17 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | >= 0.343233 J/cm @Thickness 6.40 - 6.40 mm |
>= 0.643016 ft-lb/in @Thickness 0.252 - 0.252 in |
Average value: 0.537 J/cm Grade Count:17 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |