Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.176 J/cm | 0.330 ft-lb/in | X, Y direction; ASTM D256A |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Izod Impact, Notched | 0.176 J/cm | 0.330 ft-lb/in | ASTM D256A |
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications Product Description: A homopolymer resin based on Exxpol™ metallocene technology designed for medical, electronics and other applications requiring cleanliness. It provides lower, volatiles and ext.. |
|||
Izod Impact, Notched | 0.176 - 7.26104 J/cm @Temperature -30.0 - 4.00 °C |
0.330 - 13.6029 ft-lb/in @Temperature -22.0 - 39.2 °F |
Average value: 0.794 J/cm Grade Count:56 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |