Polymer Property : Izod Impact, Notched = 0.314 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.314 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.588 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID GP3400B(W) PA66+MF40%, General Purpose
Feature: Injection Molding, PA66+MF40%, General PurposeApplication: Automotive (Engine Cover)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched 0.314 J/cm
0.588 ft-lb/in
ASTM D256
E-Polymers SEPAZ® N1040 Nanoclay 4% High Flow Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Izod Impact, Notched 0.314 J/cm
0.588 ft-lb/in
ASTM D256
E-Polymers SEPAZ® N1140 Nanoclay 4% Medium Viscosity Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Izod Impact, Notched 0.314 J/cm
0.588 ft-lb/in
ASTM D256
Cheng Yu Plastic FV30715 POM, 15% Mineral Reinforced