Polymer Property : Izod Impact, Notched = 0.310 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.166 - 0.310 J/cm
0.311 - 0.581 ft-lb/in
Average value: 0.220 J/cm Grade Count:20
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..