Polymer Property : Izod Impact, Notched = 0.275 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched >= 0.275 J/cm

@Thickness 6.35 mm
>= 0.514 ft-lb/in

@Thickness 0.250 in
ASTM D256
Gromax CCP PBT 1100-630S
Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Izod Impact, Notched >= 0.275 J/cm

@Thickness 6.35 mm
>= 0.514 ft-lb/in

@Thickness 0.250 in
ASTM D256
Gromax CCP PBT 1100-104S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Izod Impact, Notched 0.275 J/cm
0.514 ft-lb/in
ASTM D256
Cheng Yu Plastic PP230H TALC 30 Polypropylene, 30% Talc, High Heat