Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.180 - 0.267 J/cm @Temperature -20.0 - 0.000 °C |
0.337 - 0.500 ft-lb/in @Temperature -4.00 - 32.0 °F |
Average value: 0.215 J/cm Grade Count:4 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |