Mechanical Properties Metric English Comments
Izod Impact, Notched 0.190 - 0.240 J/cm
0.356 - 0.450 ft-lb/in
ASTM D256
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu..
Izod Impact, Notched 0.190 - 0.240 J/cm
0.356 - 0.450 ft-lb/in
ASTM D256
3D Systems Accura® 25 Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el..