Polymer Property : Izod Impact, Notched = 0.239 J/cm
Polymer Property :
Izod Impact, Notched =
0.239 J/cm
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Notched
0.239
J/cm
0.448
ft-lb/in
ASTM D256-06
Objet FullCure® 870 Vero Black Resin for Rapid Prototyping
Information provided by American Precision Prototyping, LLC